Home / Our Trusted Partners / CFlo / Micrograder
Micrograder silica sand washing plant
Silica sand, glass sand and foundry sand washed and graded to a narrow band, with iron and fines held where the customer wants them.
The Micrograder scrubs, screens and classifies silica sand to a specified grading band, removes iron-bearing coatings from the grains and keeps the fines within the limit.
- Feed
- Silica sand, glass sand, foundry sand, china clay by-product sand
- Products
- Glass sand, foundry sand to an AFS fineness number, filtration media, specification sand
- Process
- Attrition scrubbing, fine screening, hydrocyclone classification, dewatering
- Reference
- Float glass sand at 99.3% SiO2
- Water
- Up to 95% recycled
- Delivery
- Modular, shipped in containers
What it does
Attrition scrubbing removes coatings from the grains. Fine screens and hydrocyclones set the cut points. Dewatering screens deliver a product ready to stockpile. Where the iron content must be lower still, magnetic separation and Spiropure spirals are added as Process Modules on the same flowsheet.
Where it fits in the UK
- Glass sand producers supplying a narrow grading band for float and container glass.
- Foundry sand graded to an AFS fineness number.
- China clay operations recovering saleable sand from their by-product.
- Filtration and sports sand graded to size.
Micrograder plants running
More films: the Micrograder playlist on CFlo's YouTube channel.
Sizing and supply
A Sample Study of your sand reports the products recovered, their grading and their chemistry. CFlo then prepares the flowsheet, mass balance, layout and equipment list. Duo installs and supports the plant.
Full specification on cfloworld.com: Micrograder for the UK.
Frequently asked questions
What materials can the Micrograder process?
Silica sand, glass sand, foundry sand and sand recovered from china clay by-product.
Can the Micrograder reduce iron content in silica sand?
Yes. Attrition scrubbing removes iron-bearing coatings from the grains. Where the iron content must be lower still, magnetic separation and Spiropure spirals are added as Process Modules on the same flowsheet.
Can it produce foundry sand to an AFS fineness number?
Yes. Fine screens and hydrocyclones set the cut points, so foundry sand can be graded to a specified AFS fineness number.
What purity has a Micrograder achieved?
A reference plant produces float glass sand at 99.3% SiO2. For your sand, the Sample Study reports the products recovered, their grading and their chemistry.
Tell us your material and tonnage
Send Duo a description of the feed, the tonnage you need and the site. CFlo tests the material first. Duo quotes the plant, installs it and supports it.
CFlo and the CFlo mark are registered trade marks of CFlo World Limited. Plants are CE and UKCA marked. CFlo is a registered trade mark in the United Kingdom and the European Union, and CFlo's wet processing platforms are built on patented technology.